TiN

¡@

Coating Color Golden Yellow

tin.jpg (9453 bytes)

Hardness HV 2200
Coating Thickness 1-4um
Friction Coefficient 0.4
Max Coating Temperature 450 ºC
Max Working Temperature 600 ºC
What's the coating use for Resistance to abrasive wear, Resistance to adhesive wear, Resistance to tribooxidation
Application Injection Mold¡BCutting Tool¡BEndmill¡BDrill¡BTaps¡BHob¡BPunch & Die for fasten & Nut industrial¡BCD-R Mold¡C